MIROGARD® plus

SCHOTT MIROGARD® is an anti-reflective, completely transparent glass for use in glazing pictures. The additional versions MIROGARD® plus and MIROGARD® protect also provide increased UV protection. It minimizes reflections to less than 1% and provides art lovers with an unrestricted view. The ideal invisible protection.

Advantages:

  • Anti-reflective coating
  • High transmission
  • Neutral in color
  • Best possible color rendering index of Ra=100
Article T
H
W
sqm.
Sides coated
Reflect. Color
Cont./Box (pcs.)
Cont./Box (sqm.)
General Description

SCHOTT MIROGARD® vs. conventional Float Glass

MIROGARD® glass reduces reflections in the visible spectrum to under 1% and thus allows for an unadulterated view of art.


 MIROGARD®MIROGARD® plusMIROGARD® ProtectMIROGARD® Protect Ultra
Reflectance
ρvA %
~ 0.9%~ 1.1%~ 0.9%~ 0.9%
Transmittance
τvA %
~ 99%~ 98%~ 98%~ 98%
Mechanical protection effectlowlowmedium
to high
medium
to high
Splinter protection
UV Protection
(300 – 380 nm)
~ 48%~ 82%~ 99%~ 99%

Coating durability

SCHOTT makes an enormous technical effort to provide a nearly reflection-free view: MIROGARD® anti-reflective glass is dip-coated using the sol-gel process.

All products have passed the following tests:
- copper chloride acetic acid spray test