MIROGARD® Protect

SCHOTT MIROGARD® is an anti-reflective, completely transparent glass for use in glazing pictures. The additional versions MIROGARD® Plus and MIROGARD® Protect also provide increased UV protection. It minimizes reflections to less than 1% and provides art lovers with an unrestricted view. The ideal invisible protection.
The dimensions given are usually net dimensions without dipping edge. The gross dimension is supplied including the dipping edge.
Advantages:
- Anti-reflective coating
- Splinter protection
- Outstanding UV protection: 99.9%
- High mechanical stability
- Best possible color rendering index of Ra=100
物品编号 |
厚度 |
H |
宽度 |
sqm. |
两面涂层 |
反射色 |
片数/箱 |
m2/箱 |
---|
一般说明
SCHOTT MIROGARD® vs. conventional Float Glass
MIROGARD® glass reduces reflections in the visible spectrum to under 1% and thus allows for an unadulterated view of art.
Coating durability
SCHOTT makes an enormous technical effort to provide a nearly reflection-free view: MIROGARD® anti-reflective glass is dip-coated using the sol-gel process.
All products have passed the following tests:
- copper chloride acetic acid spray test
- sliding abrasion with Taber Abraser process
- adhesive tape test
- alcohol rubbing test
- stylus test