BG62

- SCHOTT
- BG62 - BG62
- 厚度
- 1.0
- 反射系数
- 0.9150
λ [nm] | |
---|---|
200 | |
210 | |
220 | |
230 | |
240 | |
250 | |
260 | |
270 | |
280 | |
290 | |
300 | |
310 | |
320 | < 10⁻³ |
330 | 0.005 |
340 | 0.080 |
350 | 0.261 |
360 | 0.438 |
370 | 0.559 |
380 | 0.636 |
390 | 0.686 |
400 | 0.724 |
410 | 0.755 |
420 | 0.782 |
430 | 0.805 |
440 | 0.826 |
450 | 0.846 |
460 | 0.862 |
470 | 0.876 |
480 | 0.888 |
490 | 0.897 |
λ [nm] | |
---|---|
500 | 0.901 |
510 | 0.900 |
520 | 0.890 |
530 | 0.870 |
540 | 0.836 |
550 | 0.786 |
560 | 0.718 |
570 | 0.633 |
580 | 0.536 |
590 | 0.435 |
600 | 0.335 |
610 | 0.245 |
620 | 0.169 |
630 | 0.112 |
640 | 0.069 |
650 | 0.041 |
660 | 0.023 |
670 | 0.013 |
680 | 0.007 |
690 | 0.003 |
700 | 0.002 |
710 | < 10⁻³ |
720 | < 10⁻³ |
730 | < 10⁻³ |
740 | < 10⁻³ |
750 | < 10⁻³ |
760 | < 10⁻³ |
770 | < 10⁻³ |
780 | < 10⁻³ |
790 | < 10⁻³ |
λ [nm] | |
---|---|
800 | < 10⁻³ |
810 | < 10⁻³ |
820 | < 10⁻³ |
830 | < 10⁻³ |
840 | < 10⁻³ |
850 | < 10⁻³ |
860 | < 10⁻³ |
870 | < 10⁻³ |
880 | < 10⁻³ |
890 | < 10⁻³ |
900 | < 10⁻³ |
910 | < 10⁻³ |
920 | < 10⁻³ |
930 | < 10⁻³ |
940 | < 10⁻³ |
950 | < 10⁻³ |
960 | < 10⁻³ |
970 | < 10⁻³ |
980 | < 10⁻³ |
990 | < 10⁻³ |
1,000 | < 10⁻³ |
1,010 | < 10⁻³ |
1,020 | < 10⁻³ |
1,030 | < 10⁻³ |
1,040 | < 10⁻³ |
1,050 | < 10⁻³ |
1,060 | < 10⁻³ |
1,070 | < 10⁻³ |
1,080 | < 10⁻³ |
1,090 | < 10⁻³ |
λ [nm] | |
---|---|
1,100 | < 10⁻³ |
1,110 | < 10⁻³ |
1,120 | 0.001 |
1,130 | 0.001 |
1,140 | 0.002 |
1,150 | 0.002 |
1,160 | 0.003 |
1,170 | 0.003 |
1,180 | 0.004 |
1,190 | 0.005 |
1,200 | 0.006 |
1,250 | 0.014 |
1,300 | 0.029 |
1,350 | 0.055 |
1,400 | 0.094 |
1,450 | 0.147 |
1,500 | 0.211 |
1,550 | 0.283 |
1,600 | 0.359 |
1,650 | 0.433 |
1,700 | 0.503 |
1,750 | 0.569 |
1,800 | 0.627 |
1,850 | 0.678 |
1,900 | 0.722 |
1,950 | 0.760 |
2,000 | 0.793 |
2,050 | 0.820 |
2,100 | 0.843 |
2,150 | 0.862 |
λ [nm] | |
---|---|
2,200 | 0.876 |
2,250 | 0.886 |
2,300 | 0.896 |
2,350 | 0.905 |
2,400 | 0.913 |
2,450 | 0.918 |
2,500 | 0.919 |
2,550 | 0.921 |
2,600 | 0.921 |
2,650 | 0.921 |
2,700 | 0.918 |
2,750 | 0.907 |
2,800 | 0.858 |
2,850 | 0.770 |
2,900 | 0.689 |
2,950 | 0.627 |
3,000 | 0.575 |
3,050 | 0.529 |
3,100 | 0.485 |
3,150 | 0.443 |
3,200 | 0.406 |
3,250 | 0.375 |
3,300 | 0.349 |
3,350 | 0.328 |
3,400 | 0.313 |
3,450 | 0.304 |
3,500 | 0.300 |
3,550 | 0.303 |
3,600 | 0.312 |
3,650 | 0.326 |
λ [nm] | |
---|---|
3,700 | 0.345 |
3,750 | 0.362 |
3,800 | 0.365 |
3,850 | 0.342 |
3,900 | 0.300 |
3,950 | 0.252 |
4,000 | 0.194 |
4,050 | 0.123 |
4,100 | 0.068 |
4,150 | 0.035 |
4,200 | 0.019 |
4,250 | 0.013 |
4,300 | 0.012 |
4,350 | 0.013 |
4,400 | 0.012 |
4,450 | 0.010 |
4,500 | 0.008 |
4,550 | 0.006 |
4,600 | 0.006 |
4,650 | 0.008 |
4,700 | 0.013 |
4,750 | 0.020 |
4,800 | 0.030 |
4,850 | 0.042 |
4,900 | 0.055 |
4,950 | 0.072 |
5,000 | 0.092 |
5,050 | 0.111 |
5,100 | 0.125 |
5,150 | 0.132 |
反射系数 | |
---|---|
Pd | 0.915 |
参考厚度 | |
---|---|
d [mm] | 1 |
承诺光谱值 | |
---|---|
τi (405nm) | ≥0.73 |
τi (514nm) | ≥0.89 |
τi (633nm) | ≥0.08 |
τi (694nm) | ≤0.005 |
τi (1060nm) | ≤0.0005 |
折射率 n |
---|
nF (486.1 nm) = 1.546 |
nh (404.7 nm) = 1.554 |
ng (435.8 nm) = 1.550 |
ns (852.1 nm) = 1.533 |
ne (546.1 nm) = 1.542 |
nd (587.6 nm) = 1.540 |
色度评估
光源 | A(Planck T = 2347K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | 0.321 | 0.257 | 0.220 |
y | 0.441 | 0.447 | 0.445 |
Y | 52 | 36 | 27 |
λd [nm] | 499 | 498 | 498 |
Pe | 0.29 | 0.44 | 0.52 |
光源 | Planck T = 3200 K | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | 0.302 | 0.243 | 0.210 |
y | 0.422 | 0.423 | 0.419 |
Y | 53 | 38 | 29 |
λd [nm] | 498 | 497 | 496 |
Pe | 0.30 | 0.44 | 0.53 |
光源 | D65 (TC = 6504 K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | 0.229 | 0.194 | 0.175 |
y | 0.320 | 0.311 | 0.305 |
Y | 60 | 45 | 36 |
λd [nm] | 490 | 490 | 489 |
Pe | 0.31 | 0.45 | 0.52 |
密度 | |
---|---|
p [g/cm3] | 2.848 |
气泡含量 | |
---|---|
气泡等级 |
玻转温度 | |
---|---|
Tg [°C] | 410 |
温度系数 | |
---|---|
Tk [nm/°C] |
耐化学性 | |
---|---|
耐污性 | 1 |
耐酸性 | 52.3 |
耐碱性 | 3.3 |
热膨胀 | |
---|---|
α-30°C/+70°C [10-6/K] | 11.92 |
α20°C/300°C [10-6/K] | 13.62 |
α20°C/200°C [10-6/K] |